EMAIL US  info@rotarykilnfactory.com  for FREE quotation!

Welding Flux

What is Welding Flux?

Welding flux is a crucial consumable used in the submerged arc welding (SAW) process. It is a granular auxiliary material that protects the metal and removes oxides. During welding, the flux covers the arc and the surface of the molten pool, forming a protective layer under high-temperature conditions. This effectively excludes atmospheric oxygen and nitrogen, preventing oxidation and contamination of the weld, thereby enhancing weld quality and performance.

Industrial Welding Flux

In the manufacturing sectors for rotary kilns, ball mills, pressure vessels, mining equipment, and large-scale steel structures, submerged arc welding flux is widely adopted due to its high efficiency, deep penetration, and consistent weld quality. The high-quality welding flux used in conjunction not only boosts welding efficiency but also effectively extends equipment service life and reduces long-term maintenance costs.

AGICO offers two main product lines—fused welding flux and agglomerated welding flux—suitable for a wide range of applications, including rotary kiln shell fabrication, shell crack repair, tire overlay welding, large gear ring repair welding, and various heavy equipment maintenance projects, thereby providing industrial clients with reliable welding consumable solutions.

Common Rotary Kiln Welding Repair Applications

Common Rotary Kiln Welding Repair Applications

Rotary kilns operate continuously under high temperatures, heavy loads, and demanding working conditions. Over time, key components are subjected to a combination of thermal stress, mechanical stress, and wear, which may result in cracks, surface wear, or structural deformation. By combining professional welding techniques with high-quality welding flux, damaged components can be effectively repaired, equipment performance restored, service life extended, and costly downtime minimized.

Rotary Kiln Shell Crack Repair

Prolonged exposure to thermal stress and mechanical loads can cause localized shell cracks, weld seam failures, and metal fatigue in rotary kilns.

Using professional welding processes such as submerged arc welding (SAW) together with high-quality welding flux, damaged areas can be repaired and reinforced to restore the rotary kiln shell‘s structural strength and stability. This helps prevent further crack propagation and ensures the safe and reliable operation of the equipment.

Want more details?

Contact us today to learn How to choose the right Welding Flux.

Rotary Kiln Tyre Hardfacing and Repair

The rotary kiln tyre is a critical load-bearing component that supports a significant portion of the kiln’s weight. During continuous operation, it remains in constant contact with the support rollers, making it susceptible to surface wear, localized depressions, and dimensional changes over time.

Hardfacing repair restores the worn surface by depositing a new layer of wear-resistant metal, rebuilding the tyre’s original dimensions and working surface while improving its wear resistance and load-bearing capacity.

Girth Gear Welding Repair

As the core component of the rotary kiln drive system, the girth gear is continuously subjected to high torque and impact loads. Over extended operation, gear tooth wear, root cracks, and localized tooth damage may occur, affecting the reliability and efficiency of the transmission system.

For minor to moderate damage, welding repair can be used to rebuild the affected areas, restoring the gear profile and ensuring reliable transmission performance.

Heavy Steel Structure Welding

Heavy Steel Structure Welding

In addition to rotary kiln components, steel structures such as kiln support frames, foundation structures, conveyor frames, and maintenance platforms also require extensive welding during fabrication and maintenance.

Submerged arc welding (SAW), combined with the appropriate welding flux, provides deep weld penetration and high deposition efficiency. It is particularly suitable for thick steel plates, large structural components, and heavy-duty fabrications, helping improve welding productivity while ensuring consistent weld quality.

Types of Welding Flux Supplied by AGICO

Fused Welding Flux

HJ131 Fused Welding Flux
HJ131 Fused Welding Flux
HJ330 Fused Welding Flux
HJ330 Fused Welding Flux
ModelFlux TypeAppearanceParticle SizeCurrent & PolarityKey FeaturesApplications
HJ131Manganese-free, high-silica, low-fluorideWhite to gray, pumice-like granules10–60 mesh (2.0–0.28 mm)AC or DCGood welding performanceThin nickel-alloy structures; aerospace components
HJ330Medium-manganese, high-silicaReddish-brown, glassy granules8–40 mesh (2.5–0.45 mm)AC or DC; electrode positive for DCGood weld bead appearanceLow-carbon and selected low-alloy steels; boilers and pressure vessels
HJ420High-manganese, high-silica, low-fluoride—Standard: 8–40 mesh; fine: 18–150 meshAC or DC; electrode positive for DCEasy slag removal; rust tolerance and porosity resistance; fine grade for high-speed weldingLow-carbon and high-strength low-alloy steels; ships, boilers and pipelines
HJ350Medium-manganese, medium-silica, medium-fluorideBrown to pale-yellow, glassy granules8–40 mesh (2.5–0.45 mm)AC or DC; electrode positive for DCEasy slag removal; good weld bead appearanceLow-alloy steels; ships, boilers and high-pressure vessels
HJ260Low-manganese, high-silica, medium-fluorideGray, glassy granules10–60 mesh (2.0–0.28 mm)DC; electrode positiveStable arc; good weld bead appearanceAcid-resistant stainless steel welding; roll surfacing
HJ250GLow-manganese, medium-silica, medium-fluoridePale-yellow to light-green, jade-like granules10–40 mesh (2.0–0.45 mm)DC; electrode positiveEasy slag removal; good low-temperature toughness with suitable wireHigh-strength low-alloy steels; 09Mn2V steel for service at −70°C
HJ107Manganese-free, medium-silica, medium-fluorideBlue-gray to dark-gray, pumice-like granules10–60 mesh (2.0–0.28 mm)DC; electrode positiveShallow penetration; easy slag removal; low carbon pickup and chromium lossStainless steel welding; corrosion-resistant overlays; high-manganese steel repair

Note: “—” indicates information not provided on the source page. Use a suitable welding wire for the intended application.

Want more details?

Contact us today to learn How to choose the right Welding Flux.

Agglomerated Welding Flux

SJ102D Agglomerated Welding Flux
SJ102D Agglomerated Welding Flux
SJ641 Agglomerated Welding Flux
SJ641 Agglomerated Welding Flux
ModelFlux TypeAppearanceParticle SizeCurrent & PolarityKey FeaturesApplications
SJ102DAluminate-basic—10–40 mesh—Stable arc; deposits resist thermal fatigue, high-temperature oxidation and wearWear- and impact-resistant surfacing; blast furnace bells and rolls
SJ641BasicGray-white granules10–60 mesh (2.0–0.28 mm)DC; electrode positiveStable arc; easy slag removal; suitable for titanium-bearing stainless steelsAustenitic stainless steels; low-temperature marine structures; acid-resistant structures
SJ601Basic; basicity approx. 1.8Gray-white, round granules10–60 mesh (2.0–0.28 mm)DC; electrode positiveMinimal carbon pickup; low chromium loss; good intergranular corrosion resistanceLow-carbon and ultra-low-carbon stainless steels; high-alloy heat-resistant steels
SJ501YAcidicYellow, round granules10–60 mesh (2.0–0.28 mm)AC or DC; electrode positive for DCStable arc; easy slag removal; current up to 1000 ALow-carbon and selected low-alloy steels; fine-wire welding at speeds up to 110 m/h
SJ501Aluminate-rutile, acidic; basicity 0.5–0.8Brown, round granules10–60 mesh (2.0–0.28 mm)AC or DC; electrode positive for DCEasy slag removal; porosity resistance; tolerates light rust and mill scale; up to 1000 ALow-carbon and selected low-alloy steels; multi-wire welding at approx. 110 m/h; single-pass welding on each side
SJ303Calcium-silicate—10–60 mesh (2.0–0.28 mm)DC; strip electrode positiveStable arc; easy slag removal; flat, smooth weld beadsSubmerged arc strip cladding of stainless steel transition layers; strip width <75 mm
SJ205Aluminate-basic—10–40 mesh (2.0–0.45 mm)DC; electrode positiveStable arc; easy slag removal; low diffusible hydrogen in deposited metalLow-temperature pressure vessels, offshore platforms and ships; tandem and multi-wire welding
SJ114DFluoride-basic—10–40 mesh (2.0–0.45 mm)DCStable arc; easy slag removal; good crack resistanceWear-resistant roll surfacing with suitable flux-cored wires